Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.47 µm/m-°C @Temperature 20.0 - 300 °C |
6.928 µin/in-°F @Temperature 68.0 - 572 °F |
|
Industeel CLC 1.2311 Prehardened Mold Steel (300HB/30HRC) Description: CLC 1.2311 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, carbon and manganese additions are optimized to have a fully martens.. |
|||
CTE, linear | 12.47 µm/m-°C @Temperature 20.0 - 300 °C |
6.928 µin/in-°F @Temperature 68.0 - 572 °F |
|
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability Description: CLC 1.2312 is a chromium-manganese-molybdenum grade designed for plastic mold industry. This grade is normally delivered in a prehardened condition at a hardness level of 300HB/32HRC. T.. |
|||
CTE, linear | 12.47 µm/m-°C @Temperature 200 °C |
6.928 µin/in-°F @Temperature 392 °F |
|
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |
|||
CTE, linear | 12.47 µm/m-°C @Temperature 25.0 - 92.0 °C |
6.928 µin/in-°F @Temperature 77.0 - 198 °F |
Mean |
Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy Data provided by the manufacturer, Special Metals. |