CTE, linear 12.47 µm/m-°C

@Temperature 20.0 - 300 °C
6.928 µin/in-°F

@Temperature 68.0 - 572 °F
Industeel CLC 1.2311 Prehardened Mold Steel (300HB/30HRC)
Description: CLC 1.2311 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, carbon and manganese additions are optimized to have a fully martens..
CTE, linear 12.47 µm/m-°C

@Temperature 20.0 - 300 °C
6.928 µin/in-°F

@Temperature 68.0 - 572 °F
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability
Description: CLC 1.2312 is a chromium-manganese-molybdenum grade designed for plastic mold industry. This grade is normally delivered in a prehardened condition at a hardness level of 300HB/32HRC. T..
CTE, linear 12.47 µm/m-°C

@Temperature 200 °C
6.928 µin/in-°F

@Temperature 392 °F
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy
INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL..
CTE, linear 12.47 µm/m-°C

@Temperature 25.0 - 92.0 °C
6.928 µin/in-°F

@Temperature 77.0 - 198 °F
Mean
Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy
Data provided by the manufacturer, Special Metals.