Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 23.4 - 24.4 µm/m-°C @Temperature 20.0 - 300 °C |
13.0 - 13.6 µin/in-°F @Temperature 68.0 - 572 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |