Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.05 µm/m-°C @Temperature 24.0 - 538 °C |
7.250 µin/in-°F @Temperature 75.2 - 1000 °F |
|
Latrobe Lesco 53 VIM-VAR Premium Carburizing Steel LESCO 53 VIM-VAR is a premium quality alloy carburizing gear steel designed to resist softening at elevated service temperatures. It is double vacuum processed by vacuum induction melting followed .. |
|||
CTE, linear | 13.05 µm/m-°C @Temperature 24.0 - 538 °C |
7.250 µin/in-°F @Temperature 75.2 - 1000 °F |
|
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties Data provided by Carpenter Technology Corporation.This is a carburizing steel possessing good temper resistance and high case hot hardness while maintaining high core impact strength and fracture to.. |