Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe Lesco 53 VIM-VAR Premium Carburizing Steel

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel
Manufacturer Latrobe Steel
Trade Name Lesco
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe Lesco 53 VIM-VAR Premium Carburizing Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LESCO 53 VIM-VAR is a premium quality alloy carburizing gear steel designed to resist softening at elevated service temperatures. It is double vacuum processed by vacuum induction melting followed by vacuum arc remelting to provide optimum metallurgical quality. Based on its combination of high-temperature performance, deep hardenability, and excellent toughness and fatigue resistance, Lesco 53 VIM-VAR find application in demanding helicopter and aerospace drive train components.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 35
35
Core between 70°F and 600°F
55
55
Case at 600°C
Tensile Strength, Ultimate 1170 MPa
170000 psi
Tensile Strength, Yield 965 MPa
140000 psi
Elongation at Break 16 %
16 %
in 2"
Reduction of Area 63.5 %
63.5 %
Charpy Impact 118 - 129 J
87.0 - 95.1 ft-lb
V-Notch
Thermal Properties Metric English Comments
CTE, linear 11.26 µm/m-°C

@Temperature 24.0 - 93.0 °C
6.256 µin/in-°F

@Temperature 75.2 - 199 °F
12.25 µm/m-°C

@Temperature 24.0 - 316 °C
6.806 µin/in-°F

@Temperature 75.2 - 601 °F
13.05 µm/m-°C

@Temperature 24.0 - 538 °C
7.250 µin/in-°F

@Temperature 75.2 - 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 0.11 %
0.11 %
Chromium, Cr 1.0 %
1.0 %
Copper, Cu 2.0 %
2.0 %
Iron, Fe 90.24 %
90.24 %
Manganese, Mn 0.40 %
0.40 %
Molybdenum, Mo 3.25 %
3.25 %
Nickel, Ni 2.0 %
2.0 %
Silicon, Si 0.90 %
0.90 %
Vanadium, V 0.10 %
0.10 %