Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 30.4 - 32.4 µm/m-°C @Temperature 0.000 - 50.0 °C |
16.9 - 18.0 µin/in-°F @Temperature 32.0 - 122 °F |
ASTM E831-00 |
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure DescriptionNanoTool produces strong, stiff, high temperature resistant composite parts on conventional stereolithography machines. This third generation of Somos® ProtoComposite materials is heavi.. |