Polymer Property : CTE, linear = 32.4 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 30.4 - 32.4 µm/m-°C

@Temperature 0.000 - 50.0 °C
16.9 - 18.0 µin/in-°F

@Temperature 32.0 - 122 °F
ASTM E831-00
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure
DescriptionNanoTool produces strong, stiff, high temperature resistant composite parts on conventional stereolithography machines. This third generation of Somos® ProtoComposite materials is heavi..