Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 18.0 µm/m-°C @Temperature 0.000 - 140 °C |
10.0 µin/in-°F @Temperature 32.0 - 284 °F |
X-, Y-Direction; ASTM D3386 |
Rogers Corporation TMM® TMM6 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 0.000 - 150 °C |
10.0 µin/in-°F @Temperature 32.0 - 302 °F |
X-Direction; IPC-TM-650 2.1.41 |
Rogers Corporation XT/duroid™ 8000 Thermoplastic Laminate, Circuit Material XT/duroid™ 8000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 8000 circuit materials ar.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 500 °C |
10.0 µin/in-°F @Temperature 932 °F |
|
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 500 °C |
10.0 µin/in-°F @Temperature 932 °F |
|
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 500 °C |
10.0 µin/in-°F @Temperature 932 °F |
|
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 300 °C |
10.0 µin/in-°F @Temperature 572 °F |
|
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 500 °C |
10.0 µin/in-°F @Temperature 68.0 - 932 °F |
|
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 500 °C |
10.0 µin/in-°F @Temperature 68.0 - 932 °F |
|
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 500 °C |
10.0 µin/in-°F @Temperature 68.0 - 932 °F |
|
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 600 °C |
10.0 µin/in-°F @Temperature 68.0 - 1110 °F |
|
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel Description: CLI SIRIUS 310 grade is a fully austenitic stainless steel containing 25% Cr, 0.6% Si and 20% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resi.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 400 °C |
10.0 µin/in-°F @Temperature 68.0 - 752 °F |
|
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel Description: CLI SIRIUS 314 grade is a fully austenitic stainless steel containing 25% Cr, 20% Ni and 1.8% Si. The alloy is designed for high temperature corrosion resistance applications even in se.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 21.1 - 982 °C |
10.0 µin/in-°F @Temperature 70.0 - 1800 °F |
|
Carlson 330 Austenitic Alloy General DescriptionCarlson Alloy 330 is a nickel-iron-chromium-silicon austenitic alloy. It combines high strength with excellent resistance to carburization and oxidation at temperatures to 2200°.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature <=649 °C |
10.0 µin/in-°F @Temperature <=1200 °F |
|
AK Steel 309S Austenitic Stainless steel AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic w.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 0.000 - 100 °C |
10.0 µin/in-°F @Temperature 32.0 - 212 °F |
x direction; IPC TM-650 2.4.24 |
Arlon CuClad 250 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate CuClad 250 uses a higher fiberglass/PTFE ratio to provide mechanical properties approaching those of conventional substrates. Better dimensional stability and lower thermal expansion in all directi.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 358 °C |
10.0 µin/in-°F @Temperature 68.0 - 676 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 5% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 316 °C |
10.0 µin/in-°F @Temperature 68.0 - 601 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 20% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 358 °C |
10.0 µin/in-°F @Temperature 68.0 - 676 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 5% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 316 °C |
10.0 µin/in-°F @Temperature 68.0 - 601 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 50% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 316 °C |
10.0 µin/in-°F @Temperature 68.0 - 601 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 60% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 316 °C |
10.0 µin/in-°F @Temperature 68.0 - 601 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 30% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 500 °C |
10.0 µin/in-°F @Temperature 68.0 - 932 °F |
|
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel Description: CLC 18-9L is a 18Cr-9Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. This k.. |