Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 230 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 230 µm/m-°C

@Temperature 22.0 - 260 °C
128 µin/in-°F

@Temperature 71.6 - 500 °F
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer  (discontinued **)
A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1..
CTE, linear 230 µm/m-°C

@Temperature 70.0 °C
128 µin/in-°F

@Temperature 158 °F
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
CTE, linear 230 µm/m-°C

@Temperature 22.0 - 260 °C
128 µin/in-°F

@Temperature 71.6 - 500 °F
DuPont Performance Polymers Kalrez® 1050LF FFKM Perfluoroelastomer
A general-purpose compound for O-rings, seals, and other parts used in chemical process industries. It has good hot water/steam, excellent amine resistance, and enhanced compression set properties...
CTE, linear 230 µm/m-°C

@Temperature 22.0 - 260 °C
128 µin/in-°F

@Temperature 71.6 - 500 °F
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer
A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen..
CTE, linear 230 µm/m-°C

@Temperature 22.0 - 260 °C
128 µin/in-°F

@Temperature 71.6 - 500 °F
DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer  (discontinued **)
A carbon black-filled compound that is similar to Compound 1050LF, except for higher hardness/modulus. Best hot water/steam resistance. Generally used in oil fields and process industry application..