DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer  (discontinued **)

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A carbon black-filled compound that is similar to Compound 1050LF, except for higher hardness/modulus. Best hot water/steam resistance. Generally used in oil fields and process industry applications where these properties coupled with good amine and general chemical resistance are requires.Data provided by DuPont Dow Elastomers.This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Physical Properties Metric English Comments
Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 86 - 96
86 - 96
ASTM D2240
Tensile Strength, Ultimate 21.7 MPa
3150 psi
ASTM D412
Elongation at Break 125 %
125 %
ASTM D412
100% Modulus 0.0169 GPa
2.45 ksi
ASTM D412
Tear Strength 4.52 kN/m
25.8 pli
Compression Set 35 %

@Temperature 204 °C
35 %

@Temperature 399 °F
70 hr at 204°C; ASTM D395B; Pellets
Thermal Properties Metric English Comments
CTE, linear 229 µm/m-°C

@Temperature 22.0 - 100 °C
127 µin/in-°F

@Temperature 71.6 - 212 °F
230 µm/m-°C

@Temperature 22.0 - 260 °C
128 µin/in-°F

@Temperature 71.6 - 500 °F
Specific Heat Capacity 0.945 J/g-°C

@Temperature 50.0 °C
0.226 BTU/lb-°F

@Temperature 122 °F
0.974 J/g-°C

@Temperature 100 °C
0.233 BTU/lb-°F

@Temperature 212 °F
1.053 J/g-°C

@Temperature 150 °C
0.2517 BTU/lb-°F

@Temperature 302 °F
Thermal Conductivity 0.170 W/m-K

@Temperature 200 °C
1.18 BTU-in/hr-ft²-°F

@Temperature 392 °F
0.180 W/m-K

@Temperature 100 °C
1.25 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.190 W/m-K

@Temperature 50.0 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 122 °F
Maximum Service Temperature, Air 288 °C
550 °F
Maximum recommended service temperature.
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+17 ohm-cm
5.00e+17 ohm-cm
Dielectric Constant 4.9

@Frequency 1000 Hz
4.9

@Frequency 1000 Hz
Dielectric Strength >= 17.7 kV/mm
>= 450 kV/in
Dissipation Factor 0.0050

@Frequency 1000 Hz
0.0050

@Frequency 1000 Hz