Thermal Properties Metric English Comments
CTE, linear 46.0 µm/m-°C

@Temperature -55.0 - 288 °C
25.6 µin/in-°F

@Temperature -67.0 - 550 °F
Z-Direction; IPC-TM-650 2.4.41
Rogers Corporation RO4003C Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil
RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf..
CTE, linear 46.0 µm/m-°C

@Temperature -55.0 - 288 °C
25.6 µin/in-°F

@Temperature -67.0 - 550 °F
Z-Direction; ASTM D3386-94
Rogers Corporation RO4534 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate
The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a..
CTE, linear 46.0 µm/m-°C

@Temperature <=150 °C
25.6 µin/in-°F

@Temperature <=302 °F
ISO E 831
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified
Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn..
CTE, linear 46.0 µm/m-°C

@Temperature 25.0 - 100 °C
25.6 µin/in-°F

@Temperature 77.0 - 212 °F
Vertical; ASTM D696
Unitika UNILATE® 1 SC PET
Antistatic gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and ot..