Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.10 µm/m-°C @Temperature 20.0 - 100 °C |
3.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck HPM 1700 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 6.10 µm/m-°C @Temperature 20.0 - 100 °C |
3.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
CTE, linear | 6.10 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.39 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG36 Band Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BC20 |
|||
CTE, linear | 6.10 µm/m-°C @Temperature 20.0 - 300 °C |
3.39 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott KG3 Short Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG1, KG4, KG5 |
|||
CTE, linear | 6.10 µm/m-°C @Temperature 20.0 - 300 °C |
3.39 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott KG1 Short Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG3, KG4, KG5 |
|||
CTE, linear | 6.10 µm/m-°C @Temperature 20.0 - 600 °C |
3.39 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C372 |
CeramTec Rubalit® 600 Alumina, 48% Rubalit® 600 is suitable for both mechanical and laser trimming and is chiefly used as the core for high-grade carbon-film resistors. |