Thermal Properties Metric English Comments
CTE, linear 6.10 µm/m-°C

@Temperature 20.0 - 100 °C
3.39 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck HPM 1700 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 6.10 µm/m-°C

@Temperature 20.0 - 100 °C
3.39 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
CTE, linear 6.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.39 µin/in-°F

@Temperature -22.0 - 158 °F
Schott BG36 Band Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BC20
CTE, linear 6.10 µm/m-°C

@Temperature 20.0 - 300 °C
3.39 µin/in-°F

@Temperature 68.0 - 572 °F
Schott KG3 Short Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG1, KG4, KG5
CTE, linear 6.10 µm/m-°C

@Temperature 20.0 - 300 °C
3.39 µin/in-°F

@Temperature 68.0 - 572 °F
Schott KG1 Short Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG3, KG4, KG5
CTE, linear 6.10 µm/m-°C

@Temperature 20.0 - 600 °C
3.39 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C372
CeramTec Rubalit® 600 Alumina, 48%
Rubalit® 600 is suitable for both mechanical and laser trimming and is chiefly used as the core for high-grade carbon-film resistors.