CTE, linear 4.70 µm/m-°C

@Temperature <=143 °C
2.61 µin/in-°F

@Temperature <=289 °F
Below Tg; ASTM D696
Victrex® Pipes™ PEEK polymer
VICTREX Pipes™ are durable, lightweight pipe and tube extruded from VICTREX® PEEK polymer which offer high temperature performance and a unique combination of properties. An excellent alternative ..
CTE, linear 4.70 µm/m-°C

@Temperature 20.0 - 200 °C
2.61 µin/in-°F

@Temperature 68.0 - 392 °F
CeramTec Alunit® Aluminum Nitride
Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its ..
CTE, linear 4.70 µm/m-°C

@Temperature 20.0 - 300 °C
2.61 µin/in-°F

@Temperature 68.0 - 572 °F
ASTM-C372
CeramTec Alunit® HS Aluminum Nitride
Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. I..
CTE, linear 4.70 µm/m-°C

@Temperature 25.0 - 400 °C
2.61 µin/in-°F

@Temperature 77.0 - 752 °F
CoorsTek ACI-Co6 Tungsten Carbide
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries
CTE, linear 4.70 µm/m-°C

@Temperature 20.0 - 300 °C
2.61 µin/in-°F

@Temperature 68.0 - 572 °F
ASTM-C372
CeramTec CeramCool® Alunit® Aluminum Nitride
CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit..