Material Notes:
Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its electrical and mechanical characteristics are similar to aluminum oxide. Alunit® HS is non-toxic and environmentally compatible, presenting no disposal problems. Alunit® HS substrates come in a variety of surface finishes: as fired, as fired superior, ground, or polished. They can be manufactured by using tape casting, dry pressing, lasering, or metallizing. Typical applications include: power electronics, IGBT modules, telecommunications, cooling devices, DCB (Direct Copper Bonding), and LEDs.
Physical Properties Metric English Comments
Density 3.33 g/cc
0.120 lb/in³
ASTM-C20
Water Absorption 0.00 %
0.00 %
ASTM-C373
Particle Size 4.0 - 5.0 µm
4.0 - 5.0 µm
Medium Grain (d50)
Mechanical Properties Metric English Comments
Modulus of Elasticity 320 GPa
46400 ksi
ASTM-F417
Flexural Strength 420 MPa
60900 psi
Bending Strength; 4-Point Method (40x4x3 mm³); ASTM-F417
Thermal Properties Metric English Comments
CTE, linear 4.70 µm/m-°C

@Temperature 20.0 - 300 °C
2.61 µin/in-°F

@Temperature 68.0 - 572 °F
ASTM-C372
5.20 µm/m-°C

@Temperature 20.0 - 600 °C
2.89 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C372
5.60 µm/m-°C

@Temperature 20.0 - 1000 °C
3.11 µin/in-°F

@Temperature 68.0 - 1830 °F
ASTM-C372
Specific Heat Capacity 0.738 J/g-°C
0.176 BTU/lb-°F
Thermal Conductivity 170 W/m-K
1180 BTU-in/hr-ft²-°F
ASTM-C408
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM-D257
Dielectric Constant 9.0

@Frequency 1.00e+6 Hz
9.0

@Frequency 1.00e+6 Hz
ASTM-C150
Dielectric Breakdown >= 16000 V

@Thickness 1.00 mm
>= 16000 V

@Thickness 0.0394 in
ASTM-D149
Descriptive Properties Value Comments
Color Translucent Medium Gray
Ra = Arithmetic Mean Roughness Value (µm) Profilometer (cutoff 0.8 mm); DIN ISO 4287