Thermal Properties Metric English Comments
CTE, linear 80.9 µm/m-°C

@Temperature 100 - 150 °C
44.9 µin/in-°F

@Temperature 212 - 302 °F
ASTM E831-12
DSM Somos® PerFORM Stereolithography Polymer, UV Postcure
PerFORM produces strong, stiff, high-temperature resistant composite parts on standard 355 nm stereolithography machines. This material’s lower viscosity makes processing parts faster. It exhibits ..