Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 80.9 µm/m-°C @Temperature 100 - 150 °C |
44.9 µin/in-°F @Temperature 212 - 302 °F |
ASTM E831-12 |
DSM Somos® PerFORM Stereolithography Polymer, UV Postcure PerFORM produces strong, stiff, high-temperature resistant composite parts on standard 355 nm stereolithography machines. This material’s lower viscosity makes processing parts faster. It exhibits .. |