Thermal Properties Metric English Comments
CTE, linear 35.0 - 45.0 µm/m-°C

@Temperature <=190 °C
19.4 - 25.0 µin/in-°F

@Temperature <=374 °F
Z-Direction; IPC-TM-650 2.4.24
Rogers Corporation Theta® MCL-HE-679G Laminate, GHA-679G Prepreg Halogen-Free, Low Dielectric Constant, High heat Resistant Multi-Layer Circuit Material
Theta® circuit materials are halogen free and have good dielectric characteristics suitable for high speed digital applications. Theta materials, in part due to their superior heat resistance, hav..