Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 19.4 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C

@Temperature <=79.0 °C
19.4 µin/in-°F

@Temperature <=174 °F
below Tg
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
CTE, linear 35.0 µm/m-°C

@Temperature -55.0 - 288 °C
19.4 µin/in-°F

@Temperature -67.0 - 550 °F
Z-Direction; IPC-TM-650 2.4.41
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil
RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf..
CTE, linear 35.0 µm/m-°C

@Temperature -55.0 - 288 °C
19.4 µin/in-°F

@Temperature -67.0 - 550 °F
Z-Direction; ASTM D3386-94
Rogers Corporation RO4535 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate
The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a..
CTE, linear 35.0 - 45.0 µm/m-°C

@Temperature <=190 °C
19.4 - 25.0 µin/in-°F

@Temperature <=374 °F
Z-Direction; IPC-TM-650 2.4.24
Rogers Corporation Theta® MCL-HE-679G Laminate, GHA-679G Prepreg Halogen-Free, Low Dielectric Constant, High heat Resistant Multi-Layer Circuit Material
Theta® circuit materials are halogen free and have good dielectric characteristics suitable for high speed digital applications. Theta materials, in part due to their superior heat resistance, hav..
CTE, linear 35.0 µm/m-°C

@Temperature 20.0 °C
19.4 µin/in-°F

@Temperature 68.0 °F
In machine direction.
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
CTE, linear 35.0 µm/m-°C

@Temperature 0.000 - 100 °C
19.4 µin/in-°F

@Temperature 32.0 - 212 °F
FD; ASTM E831
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded  
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre..
CTE, linear 35.0 µm/m-°C

@Temperature <=143 °C
19.4 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
CTE, linear 35.0 µm/m-°C

@Temperature <=143 °C
19.4 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica..
CTE, linear 35.0 µm/m-°C

@Temperature <=152 °C
19.4 µin/in-°F

@Temperature <=306 °F
Average below Tg; ISO 11359
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
CTE, linear 35.0 µm/m-°C

@Temperature <=100 °C
19.4 µin/in-°F

@Temperature <=212 °F
ISO E 830
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced
Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor..
CTE, linear 35.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
19.4 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Murpec® SP Polyetheretherketone
Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• ..
Copyright © lookpolymers.com All Rights Reserved