Thermal Properties Metric English Comments
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 - 100 °C
3.06 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck HPM 1750 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 - 100 °C
3.06 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck HPM 1760 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 - 300 °C
3.06 µin/in-°F

@Temperature 68.0 - 572 °F
H.C. Starck HPM 1801 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 - 450 °C
3.06 µin/in-°F

@Temperature 68.0 - 842 °F
H.C. Starck HPM 1810 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 - 100 °C
3.06 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet
Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the custo..
CTE, linear 5.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.06 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LASF43 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 5.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.06 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-SK5 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 °C
3.06 µin/in-°F

@Temperature 68.0 °F
Zircar Refractory Composites ZIRCAL-18 Refractory Board
Type ZIRCAL-18 Refractory Board is a high temperature calcium silicate block insulation with excellent mechanical properties and stability up to 1100°C(2000°F). Its high thermal insulating value m..
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 °C
3.06 µin/in-°F

@Temperature 68.0 °F
Zircar Refractory Composites ZIRCAL-45 Refractory Board
Type ZIRCAL-45 Refractory Board is a self supporting, high strength, rigid refractory product fabricated from calcium silicate, inert fillers and reinforcing agents. Its high structural strength com..
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 °C
3.06 µin/in-°F

@Temperature 68.0 °F
Zircar Refractory Composites ZIRCAL-95 Refractory Board
Type ZIRCAL-95 Refractory Board is produced from a combination of natural organic fibers and inert reinforcing fillers in a high density calcium silicate hydrate matrix. Designed as a substitute for..
CTE, linear 5.50 µm/m-°C

@Temperature 25.0 - 400 °C
3.06 µin/in-°F

@Temperature 77.0 - 752 °F
CoorsTek ACI-Co10 Tungsten Carbide
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries
CTE, linear 5.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.06 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LAK14 Glass
Information Provided by SCHOTT North America, Inc.