Polymer Property : CTE, linear = 5.55 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 9.99 µm/m-°C

@Temperature 24.0 - 93.0 °C
5.55 µin/in-°F

@Temperature 75.2 - 199 °F
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 468°C
Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c..
CTE, linear 9.99 µm/m-°C

@Temperature 24.0 - 93.0 °C
5.55 µin/in-°F

@Temperature 75.2 - 199 °F
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 482°C
Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c..