Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 482°C

Category Metal , Ferrous Metal , Tool Steel , Air-Hardening Steel
Manufacturer Carpenter Technology Corporation (Cartech)
Trade Name AerMet®-for-Tooling
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 482°C.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for components which require a combination of HRC 53/55 hardness with the highest toughness available.AerMet® is a registered trademark of Carpenter Technology Corporation.
Physical Properties Metric English Comments
Density 7.892 g/cc
0.2851 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 536
536
Estimated from Rockwell C for 3000 kg load, 10 mm ball Brinell measurement.
Hardness, Knoop 594
594
Estimated from Rockwell C
Hardness, Rockwell C 53.5
53.5
Hardness, Vickers 568
568
Estimated from Rockwell C
Tensile Strength, Ultimate 1965 MPa
285000 psi
Tensile Strength, Yield 1724 MPa

@Strain 0.200 %
250000 psi

@Strain 0.200 %
Elongation at Break 14 %
14 %
Reduction of Area 65 %
65 %
Modulus of Elasticity 194.4 GPa
28200 ksi
Young's Modulus
Shear Strength 1207 MPa
175100 psi
Charpy Impact 34.0 J
25.1 ft-lb
V-notch
Thermal Properties Metric English Comments
CTE, linear 9.99 µm/m-°C

@Temperature 24.0 - 93.0 °C
5.55 µin/in-°F

@Temperature 75.2 - 199 °F
10.8 µm/m-°C

@Temperature 24.0 - 260 °C
6.00 µin/in-°F

@Temperature 75.2 - 500 °F
11.57 µm/m-°C

@Temperature 24.0 - 538 °C
6.428 µin/in-°F

@Temperature 75.2 - 1000 °F
Thermal Conductivity 24.8 W/m-K

@Temperature 50.0 °C
172 BTU-in/hr-ft²-°F

@Temperature 122 °F
30.6 W/m-K

@Temperature 200 °C
212 BTU-in/hr-ft²-°F

@Temperature 392 °F
32.6 W/m-K

@Temperature 400 °C
226 BTU-in/hr-ft²-°F

@Temperature 752 °F
Component Elements Properties Metric English Comments
Carbon, C 0.23 %
0.23 %
Chromium, Cr 3.0 %
3.0 %
Cobalt, Co 13.4 %
13.4 %
Iron, Fe 71 %
71 %
as remainder
Molybdenum, Mo 1.2 %
1.2 %
Nickel, Ni 11.1 %
11.1 %