CTE, linear 105 µm/m-°C

@Temperature 23.0 - 100 °C
58.3 µin/in-°F

@Temperature 73.4 - 212 °F
Murtfeldt Murylon® B Nylon 6
Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope..