Polymer Property : CTE, linear = 6.561 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 11.81 µm/m-°C

@Temperature 21.0 - 149 °C
6.561 µin/in-°F

@Temperature 69.8 - 300 °F
Latrobe LSS™ L6 Tool Steel (ASTM L6)
TLS L6 tool steel is a versatile, oil-hardening tool steel that is characterized by very good toughness. TLS L6 tool steel is suitable for use as tools, dies, and machine parts which require a good ..