Polymer Property : CTE, linear = 7.60 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 7.60 µm/m-°C

@Temperature 20.0 - 300 °C
4.22 µin/in-°F

@Temperature 68.0 - 572 °F
H.C. Starck WCu 85/15 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
CTE, linear 7.60 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.22 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-BAK1 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.60 µm/m-°C

@Temperature 20.0 - 300 °C
4.22 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-KZFS11 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.60 µm/m-°C

@Temperature 20.0 - 300 °C
4.22 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-SK11 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.60 µm/m-°C

@Temperature 20.0 - 400 °C
4.22 µin/in-°F

@Temperature 68.0 - 752 °F
DIN EN 821-1
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
CTE, linear 7.60 µm/m-°C

@Temperature 20.0 - 200 °C
4.22 µin/in-°F

@Temperature 68.0 - 392 °F
CeramTec Ziralit Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
CeramTec's Zirconia Toughened Alumina (Ziralit) provides excellent strength, excellent temperature performance, and superior toughness. It has enhanced performance for high quantity volume productio..
CTE, linear 7.60 µm/m-°C

@Temperature 25.0 - 800 °C
4.22 µin/in-°F

@Temperature 77.0 - 1470 °F
ASTM-C372
CoorsTek ADS-995R MidFilm™ 99.5% Alumina Thick Film
Applications: thick films and lasers
CTE, linear 7.60 µm/m-°C

@Temperature 371 °C
4.22 µin/in-°F

@Temperature 700 °F
Carpenter Invar 36® Alloy, Annealed Bars and Strip
Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T..
CTE, linear 7.60 µm/m-°C

@Temperature 371 °C
4.22 µin/in-°F

@Temperature 700 °F
Carpenter Invar 36® Alloy, Cold Drawn Bars
Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T..
CTE, linear 7.60 µm/m-°C

@Temperature 371 °C
4.22 µin/in-°F

@Temperature 700 °F
Carpenter Invar 36® Alloy, Cold Rolled Strip
Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T..
CTE, linear 7.60 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.22 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LAK12 Glass
Information Provided by SCHOTT North America, Inc.