Polymer Property : CTE, linear = 70.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 70.0 - 115 µm/m-°C

@Temperature 25.0 - 100 °C
38.9 - 63.9 µin/in-°F

@Temperature 77.0 - 212 °F
ASTM D696
Polikim EFALON® C-25 PTFE, 25% Glass Filled
C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings..
CTE, linear 70.0 µm/m-°C

@Temperature 50.0 - 250 °C
38.9 µin/in-°F

@Temperature 122 - 482 °F
Z-Axis, Alpha 1; IPC-TM-650.2.4.41
Park Electrochemical Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg
The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a..
CTE, linear 70.0 µm/m-°C

@Temperature 200 - 300 °C
38.9 µin/in-°F

@Temperature 392 - 572 °F
ASTM TMA
PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole
Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. ..
CTE, linear 70.0 µm/m-°C

@Temperature >=143 °C
38.9 µin/in-°F

@Temperature >=289 °F
Average above Tg; ISO 11359
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac..
CTE, linear 70.0 µm/m-°C

@Temperature 50.0 - 175 °C
38.9 µin/in-°F

@Temperature 122 - 347 °F
Z-Axis Alpha 1; IPC-TM-650.2.4.41
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg
The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea..