Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 20.0 °C
40.0 µin/in-°F

@Temperature 32.0 - 68.0 °F
T<Tg; ASTM E831-93
Proto3000 Accura® 45HC Plastic Stereolithography (SLA) Prototyping Polymer
A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.Benefits:Fast build speed:Provides build speeds that are sign..
CTE, linear 72.0 µm/m-°C

@Temperature -40.0 - 0.000 °C
40.0 µin/in-°F

@Temperature -40.0 - 32.0 °F
ASTM E831-00
DSM Somos® WaterClear® 10120 Epoxy Resin for Stereolithography  (discontinued **)
DescriptionDSM Somos® 10120 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us..
CTE, linear 72.0 µm/m-°C

@Thickness 1.00 - 6.00 mm,
Temperature 20.0 °C
40.0 µin/in-°F

@Thickness 0.0394 - 0.236 in,
Temperature 68.0 °F
ASTM D696
CPC - Vycom CELTEC® Expanded Rigid foam PVC board
Celtec Displayboard is a foamed polyvinyl chloride (PVC) sheet whose combination of features makes it ideal for signage, exhibits, store displays, POP, Kiosks, screen printing and more. The surface..
CTE, linear 72.0 µm/m-°C

@Temperature 50.0 - 200 °C
40.0 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Ensinger TECASINT 4211 SD Polyimide, Black, Carbon Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
Extrusion; ASTM D696
Dow STRANDFOAM™ EA 1000 Polypropylene Foam
STRANDFOAM™ EA 1000 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibra..
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 20.0 °C
40.0 µin/in-°F

@Temperature 32.0 - 68.0 °F
T<Tg; ASTM E831-93
3D Systems Accura® 45HC Plastic for SLA® Systems
A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.ApplicationsHigh temperature testing:Automotive "under-the-ho..
CTE, linear 72.0 µm/m-°C

@Thickness 0.127 mm
40.0 µin/in-°F

@Thickness 0.00500 in
second heat; ASTM D 696
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear 72.0 µm/m-°C

@Thickness 0.127 mm
40.0 µin/in-°F

@Thickness 0.00500 in
second heat; ASTM D 696
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear 72.0 µm/m-°C

@Thickness 0.127 mm
40.0 µin/in-°F

@Thickness 0.00500 in
second heat; ASTM D 696
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 1; Perkin Elmer TMS-2
Aptek 6103-A/B Epoxy Encapsulant
Optoelectronic grade, reddish black encapsulant for IR LED discreets. Transparent to IR light while blocking out visible light.Part A is deep red. Part B is clear to pale yellow.Information provided..
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 1; Perkin Elmer TMS-2
Aptek 6108-PMF Epoxy Coating/Encapsulant
High temperature, rigid, electrical/electronic coating or encapsulant. Provides excellent environmental protection for continuous exposure to 220°C.Information provided by Aptek Laboratories, Inc.
CTE, linear 72.0 µm/m-°C

@Thickness 0.127 mm
40.0 µin/in-°F

@Thickness 0.00500 in
second heat; ASTM D 696
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear 72.0 µm/m-°C

@Thickness 0.127 mm
40.0 µin/in-°F

@Thickness 0.00500 in
second heat; ASTM D 696
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear 72.0 µm/m-°C

@Thickness 0.127 mm
40.0 µin/in-°F

@Thickness 0.00500 in
second heat; ASTM D 696
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear 72.0 µm/m-°C

@Thickness 0.127 mm
40.0 µin/in-°F

@Thickness 0.00500 in
second heat; ASTM D 696
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 1; Perkin Elmer TMS-2
Aptek 6108-PMF Epoxy Encapsulant and/or Potting Compound
High temperature, rigid, electrical/electronic coating or encapsulant. Provides excellent environmental protection for continuous exposure to 220°C. Also can be used as a high temperature wire varn..
CTE, linear 72.0 µm/m-°C

@Thickness 0.127 mm
40.0 µin/in-°F

@Thickness 0.00500 in
second heat; ASTM D 696
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear 72.0 µm/m-°C

@Thickness 0.127 mm
40.0 µin/in-°F

@Thickness 0.00500 in
second heat; ASTM D 696
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear 72.0 µm/m-°C

@Thickness 0.127 mm
40.0 µin/in-°F

@Thickness 0.00500 in
second heat; ASTM D 696
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear 72.0 µm/m-°C

@Thickness 0.127 mm
40.0 µin/in-°F

@Thickness 0.00500 in
second heat; ASTM D 696
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear 72.0 µm/m-°C

@Thickness 0.127 mm
40.0 µin/in-°F

@Thickness 0.00500 in
second heat; ASTM D 696
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..