Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 73.8 µm/m-°C @Temperature 30.0 - 100 °C |
41.0 µin/in-°F @Temperature 86.0 - 212 °F |
ASTM E831 |
3M Dyneon™ CCM605 PTFE, 25% Glass Filled
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
CTE, linear | 73.8 µm/m-°C @Temperature 20.0 °C |
41.0 µin/in-°F @Temperature 68.0 °F |
Vertical; ASTM D696 |
Dow STRANDFOAM™ EA 1000 Polypropylene Foam STRANDFOAM™ EA 1000 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibra.. |