Thermal Properties Metric English Comments
CTE, linear 8.10 µm/m-°C

@Temperature 26.7 - 204 °C
4.50 µin/in-°F

@Temperature 80.0 - 400 °F
with ply; ASTM D696
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 581 Quartz Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 - 30.0 °C
4.50 µin/in-°F

@Temperature 68.0 - 86.0 °F
Y-Direction
PCC-Advanced Forming Technology AlSiC-SD Metal Matrix Composite
AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements ..
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 - 800 °C
4.50 µin/in-°F

@Temperature 68.0 - 1470 °F
Misumi Steatite
MgO-SiO2Information provided by MISUMI Corporation.
CTE, linear 8.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.50 µin/in-°F

@Temperature -22.0 - 158 °F
Schott LLF1 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 - 300 °C
4.50 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-BASF2 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.50 µin/in-°F

@Temperature -22.0 - 158 °F
Schott SF1 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.50 µin/in-°F

@Temperature -22.0 - 158 °F
Schott SF6 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.50 µin/in-°F

@Temperature -22.0 - 158 °F
Schott SF6HT Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.50 µin/in-°F

@Temperature -22.0 - 158 °F
Schott UG5 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
CTE, linear 8.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.50 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LAF2 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 - 300 °C
4.50 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-LAK21 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 - 1000 °C
4.50 µin/in-°F

@Temperature 68.0 - 1830 °F
DIN EN 821-1
CeramTec Rubalit® IS 95 Alumina
Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva..
CTE, linear 8.10 µm/m-°C

@Temperature 1200 °C
4.50 µin/in-°F

@Temperature 2200 °F
ATI Wah Chang Nb/Nb Alloy C-103
This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig..
CTE, linear 8.10 µm/m-°C

@Temperature 20.0 - 1000 °C
4.50 µin/in-°F

@Temperature 68.0 - 1830 °F
Advanced Ceramics ACL 1085 (C-795) Alumina