Advanced Ceramics ACL 1085 (C-795) Alumina

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Advanced Ceramics Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Ceramics ACL 1085 (C-795) Alumina.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Advanced Ceramics Limited (ACL)
Physical Properties Metric English Comments
Density >= 3.80 g/cc
>= 0.137 lb/in³
Open Porosity 0.0 %
0.0 %
Mechanical Properties Metric English Comments
Hardness, Rockwell 45 N 79
79
Modulus of Elasticity 320 GPa
46400 ksi
Shear Strength >= 300 MPa

@Temperature 20.0 °C
>= 43500 psi

@Temperature 68.0 °F
Cross Breaking Strength
Thermal Properties Metric English Comments
CTE, linear 7.90 µm/m-°C

@Temperature 20.0 - 600 °C
4.39 µin/in-°F

@Temperature 68.0 - 1110 °F
8.10 µm/m-°C

@Temperature 20.0 - 1000 °C
4.50 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity >= 18.0 W/m-K
>= 125 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1000 °C
1830 °F
Te Value Tk1
1452 °C
2646 °F
Deflection temperature; No load indicated.
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+17 ohm-cm

@Temperature 20.0 °C
>= 1.00e+17 ohm-cm

@Temperature 68.0 °F
Dielectric Constant 9.05

@Frequency 1e+9 Hz
9.05

@Frequency 1e+9 Hz
9.1

@Frequency 9.368e+9 Hz
9.1

@Frequency 9.368e+9 Hz
9.51

@Frequency 1e+7 Hz
9.51

@Frequency 1e+7 Hz
Dielectric Strength 30.0 kV/mm

@Thickness 0.500 mm
762 kV/in

@Thickness 0.0197 in
Dissipation Factor <= 0.00010

@Frequency 1e+7 Hz
<= 0.00010

@Frequency 1e+7 Hz
<= 0.00010

@Frequency 1e+9 Hz
<= 0.00010

@Frequency 1e+9 Hz
<= 0.00030

@Frequency 9.368e+9 Hz
<= 0.00030

@Frequency 9.368e+9 Hz
Descriptive Properties Value Comments
Grain Size 8-15 µm