Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.8 µm/m-°C @Temperature 21.0 - 316 °C |
8.20 µin/in-°F @Temperature 69.8 - 601 °F |
|
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |
|||
CTE, linear | 14.8 µm/m-°C @Temperature 20.0 - 299 °C |
8.20 µin/in-°F @Temperature 68.0 - 570 °F |
|
Carlson 2205 (UNS S31803) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
CTE, linear | 14.8 µm/m-°C @Temperature 20.0 - 299 °C |
8.20 µin/in-°F @Temperature 68.0 - 570 °F |
|
Carlson 2205 (UNS S32205) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |