Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.50 µm/m-°C @Temperature 25.0 - 300 °C |
4.72 µin/in-°F @Temperature 77.0 - 572 °F |
|
Osprey Metals CE7 Al-Si Controlled Expansion Alloy Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 20.0 - 100 °C |
4.72 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck WCu 75/25 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.72 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG7 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.72 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SF11 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.72 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SF57 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 20.0 - 100 °C |
4.72 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy Inflection point 460°C. A nickel-iron controlled-expansion alloy containing 48% nickel. Its coefficient of thermal expansion is designed to match that of soft lead and soda-lime glasses. The a.. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.72 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SF57HT Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.72 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec RK 87 Alumina, 99.8% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.72 µin/in-°F @Temperature 68.0 - 1830 °F |
|
CeramTec Rubalit® 710 Alumina, 99.6% Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conduct.. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.72 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.72 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec V 679 Alumina, 99.7% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
CTE, linear | 8.50 - 9.20 µm/m-°C @Temperature 30.0 - 350 °C |
4.72 - 5.11 µin/in-°F @Temperature 86.0 - 662 °F |
|
ATI Allegheny Ludlum AL 4750™ Electrical Alloy, UNS K94800 or UNS K95000 The alloy produces good magnetic properties, wide latitude to control hysteresis loop shape via recrystallization modes. Applications for this grade range from electromechanical relay cores, to ver.. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.72 µin/in-°F @Temperature 68.0 - 1830 °F |
|
CeramTec Rubalit® A 1898 Alumina, 98% Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.72 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG24A Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |