Polymer Property : CTE, linear = 87.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 87.0 µm/m-°C

@Temperature 100 - 200 °C
48.3 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
3M Dyneon™ 1750 PTFE Powder  (discontinued **)
Type II PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r..
CTE, linear 87.0 µm/m-°C

@Temperature 100 - 200 °C
48.3 µin/in-°F

@Temperature 212 - 392 °F
ASTM D1530
3M Dyneon™ 1620 PTFE Powder  (discontinued **)
Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
CTE, linear 87.0 µm/m-°C

@Temperature 100 - 200 °C
48.3 µin/in-°F

@Temperature 212 - 392 °F
ASTM E1530
3M Dyneon™ 1641 PTFE Powder  (discontinued **)
Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
CTE, linear 87.0 µm/m-°C

@Temperature 100 - 200 °C
48.3 µin/in-°F

@Temperature 212 - 392 °F
ASTM E1530
3M Dyneon™ 1645 PTFE Powder  (discontinued **)
Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
CTE, linear 87.0 µm/m-°C

@Temperature 0.000 - 20.0 °C
48.3 µin/in-°F

@Temperature 32.0 - 68.0 °F
T<Tg; ASTM E831-93
3D Systems Accura® 40 Plastic for SLA® Systems
40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components a..