Material Notes:
Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide range of aggressive chemical agentsUltra-low friction coefficientContinuous service temperature range from cryogenic -330°F to 500°FExtremely resistant to embrittlement, aging or weatheringPTFE has rapidly become the material choice where low friction, high durability, excellent thermal resistance and chemical inertness characteristics are required.Data provided by Dyneon.
Physical Properties Metric English Comments
Density 2.15 g/cc
0.0777 lb/in³
ASTM D4894
Apparent Bulk Density 0.850 g/cc
0.0307 lb/in³
ASTM D4894
Particle Size 220 µm
220 µm
ASTM D4894
Deformation 4.0 %

@Pressure 15.00 MPa
4.0 %

@Pressure 2175 psi
Permanent; ASTM D261
7.0 %

@Time 86400 sec,
Pressure 15.00 MPa
7.0 %

@Time 24.0 hour,
Pressure 2175 psi
ASTM D261
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
Initial; ASTM D2240
58

@Time 15.0 sec
58

@Time 0.00417 hour
ASTM D2249
Tensile Strength at Break 27.6 MPa
4000 psi
ASTM D4894
Elongation at Break 350 %
350 %
ASTM D4894
Tensile Modulus 0.600 GPa
87.0 ksi
ASTM D4894
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature 30.0 - 100 °C
36.1 µin/in-°F

@Temperature 86.0 - 212 °F
ASTM E1530
87.0 µm/m-°C

@Temperature 100 - 200 °C
48.3 µin/in-°F

@Temperature 212 - 392 °F
ASTM D1530
110 µm/m-°C

@Temperature 200 - 300 °C
61.1 µin/in-°F

@Temperature 392 - 572 °F
ASTM D1530
Thermal Conductivity 0.310 W/m-K

@Temperature 100 °C
2.15 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM D1530
0.320 W/m-K

@Temperature 250 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM D1530
Shrinkage 3.0 %
3.0 %
ASTM D4894
Electrical Properties Metric English Comments
Dielectric Strength 2.50 kV/mm
63.5 kV/in
ASTM D149