Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 85.0 °C @Time 1.80e+7 sec |
185 °F @Time 5000 hour |
|
Murtfeldt Murylon® B Nylon 6 Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope.. |