Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 209.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 209.0 °C
408.2 °F
Unannealed; ASTM D648
PolyOne Nymax™ GF 1880 33 HS NATURAL Nylon 6/12, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedHeat StabilizedMolded Test Bars: (Dry as molded:Information provided by PolyOne Corporation.