Material Notes:
Description/Features:Glass Fiber ReinforcedHeat StabilizedMolded Test Bars: (Dry as molded:Information provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Filler Content 33 %
33 %
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 159 MPa
23000 psi
Type 1 - Rigids, Break, 0.2 in/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 214 MPa
31000 psi
ASTM D790
Flexural Modulus 7.24 GPa
1050 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
2.40 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 209.0 °C
408.2 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 193.0 °C
379.4 °F
Unannealed; ASTM D648