Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 226 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 - 226 °C
410 - 439 °F
Average value: 219 °C Grade Count:22
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Deflection Temperature at 0.46 MPa (66 psi) 75.0 - 226 °C
167 - 439 °F
Average value: 190 °C Grade Count:18
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..