Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 226 °C | 410 - 439 °F | Average value: 219 °C Grade Count:22 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 - 226 °C | 167 - 439 °F | Average value: 190 °C Grade Count:18 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |