Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 223 - 245 °C
433 - 473 °F
Average value: 236 °C Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep..
Deflection Temperature at 0.46 MPa (66 psi) 130 - 245 °C
266 - 473 °F
Average value: 208 °C Grade Count:60
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Deflection Temperature at 0.46 MPa (66 psi) 230 - 245 °C
446 - 473 °F
Average value: 241 °C Grade Count:21
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..