Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.25 - 1.72 g/cc
0.0452 - 0.0621 lb/in³
Average value: 1.54 g/cc Grade Count:5
Water Absorption 0.0600 - 0.0900 %
0.0600 - 0.0900 %
Average value: 0.0750 % Grade Count:4
Linear Mold Shrinkage 0.00200 - 0.0140 cm/cm
0.00200 - 0.0140 in/in
Average value: 0.00530 cm/cm Grade Count:5
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.0 - 140 MPa
9430 - 20300 psi
Average value: 105 MPa Grade Count:5
Elongation at Break 1.40 - 8.00 %
1.40 - 8.00 %
Average value: 3.24 % Grade Count:5
Flexural Yield Strength 100 - 215 MPa
14500 - 31200 psi
Average value: 160 MPa Grade Count:5
Flexural Modulus 3.70 - 15.6 GPa
537 - 2260 ksi
Average value: 9.66 GPa Grade Count:5
Izod Impact, Notched 0.380 - 0.700 J/cm
0.712 - 1.31 ft-lb/in
Average value: 0.565 J/cm Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 30.6 - 37.8 µm/m-°C
17.0 - 21.0 µin/in-°F
Average value: 32.4 µm/m-°C Grade Count:4
12.96 - 23.4 µm/m-°C

@Temperature 100 - 100 °C
7.200 - 13.0 µin/in-°F

@Temperature 212 - 212 °F
Average value: 18.2 µm/m-°C Grade Count:2
CTE, linear, Transverse to Flow 50.0 - 103 µm/m-°C
27.8 - 57.2 µin/in-°F
Average value: 78.8 µm/m-°C Grade Count:4
66.6 - 84.6 µm/m-°C

@Temperature 100 - 100 °C
37.0 - 47.0 µin/in-°F

@Temperature 212 - 212 °F
Average value: 75.6 µm/m-°C Grade Count:2
Melting Point 248 - 260 °C
478 - 500 °F
Average value: 252 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 223 - 245 °C
433 - 473 °F
Average value: 236 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 100 - 228 °C
212 - 442 °F
Average value: 184 °C Grade Count:5
Flammability, UL94 HB
HB
Grade Count:4
Electrical Properties Metric English Comments
Dielectric Constant 3.20 - 3.90
3.20 - 3.90
Average value: 3.65 Grade Count:4
Dielectric Strength 17.0 - 21.0 kV/mm
432 - 533 kV/in
Average value: 18.8 kV/mm Grade Count:4
Dissipation Factor 0.0100 - 0.0200
0.0100 - 0.0200
Average value: 0.0125 Grade Count:4
Arc Resistance 101 - 126 sec
101 - 126 sec
Average value: 120 sec Grade Count:4
Comparative Tracking Index 200 - 250 V
200 - 250 V
Average value: 217 V Grade Count:3
Processing Properties Metric English Comments
Processing Temperature 270 - 280 °C
518 - 536 °F
Average value: 275 °C Grade Count:4