Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 315 °C | 599 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp LFZ42XXC PEEK LNP THERMOCOMP* LFZ42XXC is a compound based on Polyetheretherketone resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage.This data was supplied by SABIC.. |