Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 98.9 - 182 °C | 210 - 360 °F | Average value: 147 °C Grade Count:63 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 138 - 182 °C | 280 - 360 °F | Average value: 172 °C Grade Count:22 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 - 182 °C | 185 - 360 °F | Average value: 138 °C Grade Count:24 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |