Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
Nilit FRIANYL A63 N-V2 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, low viscosity, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
Nilit FRIANYL A63 RV0 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
Nilit FRIANYL A63 S10 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
Nilit FRIANYL A63 V0 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
Nilit FRIANYL A63 V2 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | |
LATI Latistat 67-08 PA66, Impact Modified Dissipative product based on Polyamide 66 (PA66), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Lubricomp GFL14 PSU LNP* Lubricomp* GFL14 is a compound based on Polysulfone containing Glass Fiber and PTFE Lubricant.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Lubricomp GFL14 PSU LNP* Lubricomp* GFL14 is a compound based on Polysulfone containing Glass Fiber and PTFE Lubricant.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75-2 |
Solvay Technyl® C206F Unfilled, Fast Cycle Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp GF003 PSU LNP THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl GTX CRN500 PPE+PA6 (Asia Pacific) Pa6 based unfilled GTX for Non-Auto marketThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | DIN 53461 |
Polyram PlusTek PB140 Nylon 6, Injection Molding Polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BS 23 PA6 Information provided by EMS Grivory |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® XE 4185 black 9453 PA* Product description: Grivory XE 4185 is a non-reinforced heat stabilized engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation: PA 10.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
Ascend Performance Materials Vydyne® 47 Nylon 66, DAM Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75-1/-2 |
DSM Akulon® F223-DH Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Europe-Africa-Middle East) LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber. |