Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 378 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 180 - 192 °C
356 - 378 °F
Average value: 185 °C Grade Count:3
Overview of materials for Nylon 11 with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ..