Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 42.8 °C | 109 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7144 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as large industrial containers and trash cans. Information provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 42.8 °C | 109 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8320 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 42.8 °C | 109 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow GRSN-9820 NT 7 Linear Low Density Polyethylene Granular Solid DOW GRSN-9820 NT 7 is produced using UNIPOL™ PE process technology and is supplied in granular form. This resin is specifically designed as a carrier resin for color concentrates and other master .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 42.8 °C | 109 °F | ASTM D648 |
Aclo Accucomp Polyethylene LD0102L Low Density |