Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa PA66-C111 Toughened PA66 Features:High impactLow tendency to wrapExcellent balance propertiesApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C | 459 °F | ISO 75/Bf |
Solvay TECHNYL® A 50H1 PA66, DRY Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM AUT230 PEI (Europe-Africa-Middle East) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem AUT230M PEI Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 3.20 mm |
459 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C | 459 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 E4 A1 Nylon 66 Availability: North AmericaForms: PelletsFeatures: High ViscosityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C | 459 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 E4 IM Nylon 66 Availability: North AmericaForms: PelletsFeatures: Good Toughness and High ViscosityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C | 459 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/6 L UV BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: UV Stabilizer and LubricantFeatures: LubricatedAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C | 459 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM AUT230 PEI Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM AUT230 PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C | 459 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 HS MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedTPCI# 9094101Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C @Thickness 6.40 mm |
459 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
Westlake Plastics Tempalux® 5000 Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high heat resistance, high strength at elevated temperatures, hi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 237 °C | 459 °F | ISO 75-1/-2 |
DuPont Performance Polymers Rynite® 408 BK515 PET Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info.. |