Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 263 °C | 410 - 505 °F | Average value: 249 °C Grade Count:65 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 260 - 263 °C | 500 - 505 °F | ASTM D648 |
Clariant Renol PA1SP0019 Nylon 66/PPS Alloy, 20% Glass, 20% Mineral Data provided by Clariant Masterbatches |