Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 272 °C | 522 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched LNP* LUBRICOMP* OCP36A is a compound based on PPS - Branched resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 272 °C | 522 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific) LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 272 °C | 522 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 272 °C | 522 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS (Asia Pacific) LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |