Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 560 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 293 °C
560 °F
Unannealed; ASTM D648
PolyOne Therma-Tech™ SF-6000 TC Polyphenylene Sulfide (PPS)  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Deflection Temperature at 0.46 MPa (66 psi) 293 °C
560 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA4/6 CF30 TL10 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: LubricatedTPCI# 8661150Information provided by TP Composites, ..
Deflection Temperature at 0.46 MPa (66 psi) 293 °C
560 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA4/6 CF30 TL15 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance and Low FrictionInformation p..